Bayflex® MP-10000 IMR
elastomeric RIM system; processed on reaction injection molding (RIM) equipment and is used for rollers, gaskets, and encapsulated windows; density 62.4 lb/ft³; tensile strength, ultimate 2,200 lb/in²; flexural modulus 10,000 lb/in² @ 23°C (73°F)
i
Market Switch
Selection will influence the results you get.
About
Product Types
- System
Material
No data available
General Characterization
Bayflex MP-10,000 IMR is a solid elastomer which has a flexural modulus of approximately 10,000 psi (69 MPa) at room temperature.*
Storage Conditions
Bayflex MP-10,000 IMR is a formulated RIM system supplied as two liquid components. Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol. Note: Component B should be agitated thoroughly prior to transfer of contents from the drum to the day tank.
Component A (MDI prepolymer) must be stored in tightly closed containers and protected from contamination with moisture and other foreign substances, which can adversely affect processing. It will react slowly with water to form ureas and carbon dioxide gas, which may cause sealed containers to expand and rupture. The headspace of partially filled containers should be blanketed with dry nitrogen. Storage temperatures should be maintained between 24° and 30°C (75° and 86°F). Under these conditions, Component A will remain clear for up to six months. Within this range, lower storage temperatures will maximize the storage life of the product. Component A must not be allowed to freeze. Exposure to temperatures less than 15°C (59°F), even for short periods of time, can result in the formation of solid material. During the winter months, appropriate precautions must be taken during shipment and storage. Prolonged storage of solid or partially solid Component A may result in the formation of MDI dimer in amounts which exceed its solubility in the prepolymer at normal storage temperatures. This can make the product unusable.
If solids should form because of exposure of Component A to lower temperatures, it may be possible to reliquify the product by heating. Use a well-ventilated oven for the minimum time necessary to render it clear. The temperature of the product should not exceed 60°C (140°F). Agitation or drum rollers are recommended to avoid excessive local heating, which will degrade the prepolymer. Significant amounts of MDI dimer may form during the heating process. As a result, the re ... text to long! (max 2000 characters)
Component A (MDI prepolymer) must be stored in tightly closed containers and protected from contamination with moisture and other foreign substances, which can adversely affect processing. It will react slowly with water to form ureas and carbon dioxide gas, which may cause sealed containers to expand and rupture. The headspace of partially filled containers should be blanketed with dry nitrogen. Storage temperatures should be maintained between 24° and 30°C (75° and 86°F). Under these conditions, Component A will remain clear for up to six months. Within this range, lower storage temperatures will maximize the storage life of the product. Component A must not be allowed to freeze. Exposure to temperatures less than 15°C (59°F), even for short periods of time, can result in the formation of solid material. During the winter months, appropriate precautions must be taken during shipment and storage. Prolonged storage of solid or partially solid Component A may result in the formation of MDI dimer in amounts which exceed its solubility in the prepolymer at normal storage temperatures. This can make the product unusable.
If solids should form because of exposure of Component A to lower temperatures, it may be possible to reliquify the product by heating. Use a well-ventilated oven for the minimum time necessary to render it clear. The temperature of the product should not exceed 60°C (140°F). Agitation or drum rollers are recommended to avoid excessive local heating, which will degrade the prepolymer. Significant amounts of MDI dimer may form during the heating process. As a result, the re ... text to long! (max 2000 characters)
Sampling
No data available
Packaging Type
No data available
Downloads
-
Technical Data Sheet
-
Safety Data SheetNo direct download available, please visit www.productsafetyfirst.covestro.com