Applications
NeoCryl® FL-715 provide low temperature heat seal coatings on OPP packaging films exhibiting excellent antiblock and broad printability with different types of printing inks.
Form supplied
Form supplied is approximately 25 % in Water
Specification
Property | Test Condition | Value | Unit | Standard |
---|---|---|---|---|
Appearance | Translucent | GAP0059 | ||
Free monomer | max. 200 | ppm | GAP0118 | |
pH | 9,5 - 10,5 | GAP0016 | ||
Solids | 24,5 - 25,5 | % | GAP0001 | |
Viscosity | ≤ 100 | mPa·s | GAP0020 |
Typical Values
Property | Test Condition | Value | Unit | Standard |
---|---|---|---|---|
Density at 20ºC | +/- 1,05 | g/cm3 | GAP-0006 | |
MFFT | +/- 26 | ºC | GAP-0011 |
Solubility / thinnability
NeoCryl® FL-715 can be thinned with water.
Storage
The resin should be stored indoors in original, unopened and undamaged container in a dry place at storage temperature between 5- 40 °C. Exposure to direct sunlight should be avoided.
Storage time
Covestro represents that, for a period of 6 months (180 days) following the day of shipment as stated in the respective transport documents, the product will meet the specifications or values set forth in section "specifications or characteristic data" above, what ever is applicable, provided that the product is stored in full compliance with the storage conditions set forth in and referenced under section "storage" above and is otherwise handled appropriately. The lapse of the 6 months (180 days) period does not necessarily mean that the product no longer meets specifications or the set values. However, prior to using said product, Covestro recommends to test such a product if it still meets the specifications or the set values. Covestro does not make any representation regarding the product after the lapse of the 6 months (180 days) period and Covestro shall not be responsible or liable in any way for the product failing to meet specifications or the set values after the lapse of the 6 months (180 days) period.